EN 353 Round Bar

EN 353 Round Bar

Refer Specification of IS 15NiCr1Mo12 Black Bar

EN 353 Round Bar Specification

EN 353 Round Bar

ASTM Standard

EN 353 Grade Rod ASTM Standard

 Round Bar Size

EN 353 Round Bar Size

Length

Steel EN 353 Forged Bar Length

Tensile Strength

EN 353 BS970 Flat Bar Tensile Strength

Density

EN 353 Steel Square Bar Density

Hardening

BS970 EN 353 Rod Hardening

Melting Point

Steel EN 353 Rounds Melting Point

Annealing Process

EN 353 Standard Hex Bar Annealing Process

Elongation

Elongation of EN 353 Grade Steel Black Bar

Applications

EN 353 Alloy Steel Hexagonal Bar Applications

Features

EN 41B Medium Alloy Steel Hex Bar Features

Supplier of EN 353 Round Bar in India, View Temperature Range

Temperature Range of EN 353 Grade Steel Black Bar
Stress-relief annealing °C Cooling
150-200 Furnace
EN 353 Alloy Steel Hexagonal Bar Quenching
Properties Value
1st pre-heating °C up to approx. 400 in an air-circulating furnace
2nd and 3rd 780 and 850
Hardening °C 780-820
Quenching 810 °C Oil ,Quench
Tempering °C at least twice 150-200
Hardness after Teperature HRC 62 – 64
Most Common Types of EN 353 Round Bar
EN 353 Steel Cold Drawn Bar

EN 353 Steel Cold Drawn Bar

BS970 EN 353 Black Bar

BS970 EN 353 Black Bar

EN 353 Grade Steel Bright Bar

EN 353 Grade Steel Bright Bar

Steel EN 353 Rod

Steel EN 353 Rod

EN 353 Alloy Steel Forged Bar

EN 353 Alloy Steel Forged Bar

EN 353 BS970 Square Bar

EN 353 BS970 Square Bar

EN 353 Grade Hex Bar

EN 353 Grade Hex Bar

EN 353 Standard Flat Bar

EN 353 Standard Flat Bar

Check find ready stock of Steel EN 353 Forged Bar in Cut to length, refer Hardness in HRC

EN353 Material Hardness in Hrc
Properties Value
Hardness in HRC HB – 270
Find Equivalent Material of EN 353 Grade Steel Black Bar
BS970 EN 353 Hexagon Rod Equivalent Material
Standards Value
BRITISH BS 970:1991 815M17/ 970:1955 EN353
GERMAN DIN 20NiCrMo5
FRENCH AFNOR 20NCD5
SWEDISH SS 2523
EUROPEAN EN10277-4
STEEL NAME 17NiCrMoS6-4
Refer Chemical Composition & Tensile Strength of EN 353 Medium Alloy Steel Bright Bar
Chemical Composition of Steel EN 353 Forged Bar
Carbon

Carbon

0.10 – 0.20

Manganese

Manganese

0.50 – 1.00

Silicon

Silicon

0.10 – 0.35

Sulfur

Sulfur

Max 0.040

Phosphorus

Phosphorus

Max 0.040

Chromium

Chromium

0.75 – 1.25

Molybdenum

Molybdenum

0.08 – 0.15

Nickel

Nickel

1.00 – 1.50

EN 353 BS970 Flat Bar Physical Properties
Density

Density

7.85 g/cm³

Modulus of Elasticity

Modulus of Elasticity

210 GPa (30.5 x 10^6 psi)

Thermal Conductivity

Thermal Conductivity

45 W/m·K

Thermal Expansion

Thermal Expansion

11.7 x 10^-6 /°C

Melting Point

Melting Point

1425-1540°C (2600-2800°F)

Thermal Conductivity of EN 353 Grade Rod
Thermal Conductivity at °C 20 350 700
W/(m*K) 11.3 13.3 14.5
Mechanical Properties of EN 353 Steel Square Bar
Tensile Strength

Tensile Strength

80 (551)

Yield Strength

Yield Strength 0.2% Proof

35 (241)

Elongation

Elongation

30

Delivery Time & Location of EN42B Carbon Steel Square Bar
Export to Price changes and the expected delivery
Uk 5 % extra | 30 days
France 5 % extra | 30 days
Italy 5 % extra | 30 days
Malaysia 5 % extra | 10 days
Philippines 5 % extra | 14 days