EN9 Round Bar

EN9 Round Bar

Check BS 070M55 Steel Square Bar Quenching & tempering Process

EN9 Round Bar Specification

EN9 Round Bar Specification

Round Bar Sizes

EN9 Steel Round Bar Sizes

Thickness

Steel EN9 Rounds Thickness

 Square Bar Sizes

EN9 Grade Steel Square Bar Sizes

 Standard

Standard of EN9 Steel

Certificate

EN9 Medium Carbon Steel Rod Certificate

Thickness

EN9 Medium CS Square Bar Thickness

Cutting method

Cutting method of EN9 Standard

Quenching & tempering Process

Quenching & tempering Process

Applications

Applications of EN9 CS Round Bar

View EN9 Carbon Steel Hexagonal Bar Price in India, also Refer CK55 Grade Square Bar Equivalent Material

EN9 Round Bar Equivalent
BS 970 1955 EN AISI/SAE BS 970 1991 WNR
EN9 1055 070M55 1.0535
Frequently Used EN9 Round Bar
EN9 Steel Rod

EN9 Steel Rod

EN9 Grade Steel Flat Bar

EN9 Grade Steel Flat Bar

Steel EN9 Square Bar

Steel EN9 Square Bar

EN9 Medium CS Forged Bar

EN9 Medium CS Forged Bar

EN9 BS970 Bright Bar

EN9 BS970 Bright Bar

EN9 Grade Hexagon Rod

EN9 Grade Hexagon Rod

EN9 Standard Black Bar

EN9 Standard Black Bar

BS970 EN9 Hexagon Rod stock available in H8 Precision Ground Finish

Finish of EN9 BS970 Round Bar
  • Smooth turned
  • Centreless ground
  • Polish
  • Rough Turned
  • Hot rolled annealed
  • Cold (bright) drawn
  • Bright
  • Slit rolled edge
Hardness Range of EN9 Threaded Bar
Properties Value
Hardness Range 55-62
Check EN9 Standard Hex Bar Chemical Composition
EN9 Chemical Composition
Carbon

Carbon

0.17-0.24

Silicon

Silicon

0.17-0.37

Mangenese

Mangenese

0.7-1.00

Sulfur

Sulfur

≤0.035

Phosphorus

Phosphorus

≤0.035

Chromium

Chromium

≤0.25

Nickel

Nickel

≤0.25

Copper

Copper

≤0.25

Sizes in mm of EN9 Steel Bright Bar
Sizes in mm
90 280
85 220
50 140
65 160
40 125
55 150
75 190
70 180
32 120
45 130
80 200
Physical properties of EN9 Grade Steel Square Bar
Density

Density

7.85 g/cm³

Modulus of Elasticity

Modulus of Elasticity

210 GPa (30.5 x 10^6 psi)

Thermal Conductivity

Thermal Conductivity

45 W/m·K

Thermal Expansion

Thermal Expansion

11.7 x 10^-6 /°C

Melting Point

Melting Point

1425-1540°C (2600-2800°F)

Refer EN9 Medium Carbon Steel Rod Material Mechanical Properties
Steel EN9 Forged Bar Mechanical Properties
Tensile Strength

Tensile Strength (Mpa)

≥380

Yield Strength

Yield Strength (Mpa)

≥210

Elongation

Elongation in 100-150 mm(%)

≥25

Reduction

Reduction in Area

≥50

Hardness

Hardness

≤111HB

Delivery Time and Location for EN9 CS Rounds
Export to Price changes and the expected delivery
South Korea 5 % extra | 7 days
Japan 5 % extra | 7 days
Sri Lanka 5 % extra | 5 days
Maldives 5 % extra | 7 days
Bangladesh 5 % extra | 14 days